RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: ZrO2 (Zirconium dioxide, Zirconia)

Adair et al. 1989

LogX   LogY   eV

Details

Adair et al. 1989

Reference

Comments

Data




Conditions




Additional information

About Zirconium dioxide

Zirconium dioxide (ZrO2), often known as zirconia, is a white crystalline oxide of zirconium. Its most naturally occurring form, with a monoclinic crystalline structure, is the mineral baddeleyite. Zirconia is synthesized in various colors for use as a gemstone or in jewelry – cubic zirconia. The material's high melting point, chemical resistance, and low thermal conductivity make it a valuable component in various refractory applications. Additionally, its notable toughness and biocompatibility have made it a popular choice for dental ceramics and other biomedical applications, like hip implants. In optical applications, stabilized zirconia is used as a solid-state electrolyte in oxygen sensors and fuel cells due to its high oxygen ion conductivity.

Other names and variations

  • ZrO2
  • Zirconia
  • Zirconium(IV) oxide
  • Zirconium oxide

Links