n2 Explorer: ZnSe (Zinc selenide)

Polycrystalline
Matteo et al. 2024; 220 fs
Matteo et al. 2024; 200 ps
Polyanskiy et al. 2024
Jansonas et al. 2022
Patwardhan et al. 2021
Pigeon et al. 2020
Ensley and Bambha 2019
Werner et al. 2019
Sheik-Bahae et al. 1991

LogX   LogY   eV

Details

Polycrystalline
Matteo et al. 2024; 220 fs
Matteo et al. 2024; 200 ps
Polyanskiy et al. 2024
Jansonas et al. 2022
Patwardhan et al. 2021
Pigeon et al. 2020
Ensley and Bambha 2019
Werner et al. 2019
Sheik-Bahae et al. 1991