RefractiveIndex.INFO

Refractive index database


nk database   |   n2 database   |   raw data   |   about

Shelf

Book

n2 Explorer: ZnS (Zinc sulfide)

Crystal
Adair et al. 1989: (o)
Adair et al. 1989: (e)
Polycrystalline
Polyanskiy et al. 2024
Jansonas et al. 2022
Patwardhan et al. 2021
Ensley and Bambha 2019
Flom et al. 2015

LogX   LogY   eV

Details

Crystal
Adair et al. 1989: (o)
Adair et al. 1989: (e)
Polycrystalline
Polyanskiy et al. 2024
Jansonas et al. 2022
Patwardhan et al. 2021
Ensley and Bambha 2019
Flom et al. 2015

Reference

Comments

Data




Conditions




Additional information