RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: LiF (Lithium fluoride)

Ensley and Bambha 2019
DeSalvo et al. 1996
Adair et al. 1989
Milam et al. 1977

LogX   LogY   eV

Details

Ensley and Bambha 2019
DeSalvo et al. 1996
Adair et al. 1989
Milam et al. 1977

Reference

Comments

Data




Conditions




Additional information

About Lithium fluoride

Lithium fluoride (LiF) is a simple ionic compound commonly used in optics and radiation detection. It is transparent over a broad spectral range, from ultraviolet to mid-infrared wavelengths. This characteristic makes it an ideal material for specialized UV and IR windows and lenses. It also serves as a mount for samples to be studied by X-ray crystallography. One of its notable features is its high resistance to radiation damage, making it useful in environments with high-energy radiation. However, it is relatively soft and is moisture-sensitive, requiring careful handling to maintain its optical properties.

Other names and variations:
  • LiF
  • Lithium(I) fluoride
Links: