n2 Explorer: KBr (Potassium bromide)

VanderLinden et al. 2025
Polyanskiy et al. 2024
DeSalvo et al. 1996
Adair et al. 1989

LogX   LogY   eV

Details

VanderLinden et al. 2025
Polyanskiy et al. 2024
DeSalvo et al. 1996
Adair et al. 1989

Reference

Comments

Data




Conditions




Additional information

About Potassium bromide

Potassium bromide (KBr) is a salt commonly used in the form of a transparent crystal for a variety of optical applications. Its wide transmission range, extending from the ultraviolet into the far-infrared spectrum, makes it a popular choice for infrared spectroscopy. KBr is also used as a substrate material for specialized optical coatings. It is hygroscopic, meaning it readily absorbs moisture from the air, so care must be taken in its handling and storage to maintain its optical properties. It is not advisable for applications where it would be exposed to high moisture or extreme environmental conditions. Despite its hygroscopic nature, KBr is highly valued for its excellent transmission characteristics and is a staple in various optical and spectroscopic setups.

Other names and variations:
  • KBr
Links: