Optical constants of VITRON - IG
IG 5
Wavelength:
µm
(1–14.0)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=2.810945+\frac{3.046894λ^2}{λ^2-0.402147^2}+\frac{1.793191λ^2}{λ^2-46.757008^2}$$Comments
Room temperature. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.
References
1) VITRON datasheet IG-5 June 2014