Optical constants of LightPath - Infrared glass (BD)
BDNL4
Wavelength:
µm
(1–15.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
temperature: 293
Comments
20 °C.
References
BLACK DIAMOND BDNL4 Glass Datasheet (revision 2024-04-04)
Data
Additional information
Properties of BDNL4
density: - value: 4500 thermal_expansion: - value: 2.52E-5 thermal_dispersion: - type: dn/dT temperature: 295 wavelength_range: 8 12 value: -1.63E-5 - type: dn/dT temperature: 295 wavelength_range: 3 5 value: -1.43E-5 - type: dn/dT temperature: 295 wavelength_range: 1 2 value: -9.7E-6 transformation_temperature: - value: 478 thermal_conductivity: - value: 0.17 hardness: - type: Vickers value: 1480000000 youngs_modulus: - value: 14200000000