Optical constants of LightPath - Infrared glass (BD)
BD-2
Wavelength:
µm
(3–14)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
All values represent glass characteristics after molding
References
BD-2 Glass Datasheet (revision 2013-05)
Data
Additional information
Properties of BD-2
density:
-
value: 4670
hardness:
-
type: Knoop
value: 1470000000
youngs_modulus:
-
value: 22100000000
thermal_expansion:
-
value: 1.4E-5
thermal_dispersion:
-
type: dn/dT
value: 9.1E-5
transformation_temperature:
-
value: 551