Optical constants of LightPath - BD
BD6
Wavelength:
µm
(2–14)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
temperature: 293
Comments
20 °C.
References
BLACK DIAMOND BD6 Glass Datasheet (revision 2023-07-28)
See also datasheet revision 2018-03-02 for more information.
Data
Additional information
Properties of BD6
density: - value: 4630 thermal_expansion: - value: 2.25E-5 thermal_dispersion: - type: dn/dT wavelength_range: 8 12 value: 3.05E-5 transformation_temperature: - value: 458