Optical constants of LightPath - BD
BD-2
Wavelength:
µm
(3–14)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
All values represent glass characteristics after molding
References
BD-2 Glass Datasheet (revision 2013-05)
Data
Additional information
Properties of BD-2
density: - value: 4670 hardness: - type: Knoop value: 1470000000 youngs_modulus: - value: 22100000000 thermal_expansion: - value: 1.4E-5 thermal_dispersion: - type: dn/dT value: 9.1E-5 transformation_temperature: - value: 551