Optical constants of ISUZU - Optical glass filters
IUV340

Wavelength: µm
 (0.200–2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

UV transmitting filter, Visible absorbing filter (IUV series). Glass type: P2O5-Al2O3.

References

Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of IUV340

nd: 1.526
Vd: 65.7
density:
  - 
    value: 2640
thermal_expansion:
  - 
    temperature_range: 373 573
    value: 5.9E-6
transformation_temperature:
  - 
    value: 873
durability: 2
hardness:
  - 
    type: Knoop
    value: 4840000000

About Isuzu Glass Ltd.

Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.