RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of ISUZU - Optical glass filters
IEC508

Wavelength: µm
 (0.300–1.500)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Blue filter for color compensation (IEC series). Glass type: P2O5-Al2O3.

References

Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of IEC508

nd: 1.532
Vd: 53.2
density:
  - 
    value: 2640
thermal_expansion:
  - 
    temperature_range: 373 573
    value: 9.4E-6
transformation_temperature:
  - 
    value: 705
durability: 2
hardness:
  - 
    type: Knoop
    value: 4800000000

About Isuzu Glass Ltd.

Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.

Links: