Optical constants of ISUZU - IHU (UV transmitting filter)
IHU340
Wavelength:
µm
(0.200–2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
UV transmitting filter (IHU series). Glass type: P2O5-Al2O3.
References
Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products
Data
Additional information
Properties of IHU340
nd: 1.516 Vd: 73.7 density: - value: 2570 thermal_expansion: - temperature_range: 373 573 value: 5.8-06 transformation_temperature: - value: 883 durability: 1 hardness: - type: Knoop value: 4250000000
About Isuzu Glass Ltd.
Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.