Optical constants of ISUZU - IEC (Blue filter for color compensation)
IEC578
Wavelength:
µm
(0.300–1.500)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Blue filter for color compensation (IEC series). Glass type: P2O5-Al2O3.
References
Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products
Data
Additional information
Properties of IEC578
nd: "1.540" Vd: "54.0" density: - value: 2720 thermal_expansion: - temperature_range: 373 573 value: 7.0E-6 transformation_temperature: - value: 788 durability: 1 hardness: - type: Knoop value: 4990000000
About Isuzu Glass Ltd.
Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.