RefractiveIndex.INFO

Refractive index database


nk database   |   n2 database   |   about

Shelf

Book

Page

Optical constants of CARGILLE
Acrylic matching liquid

Wavelength: µm
 (0.31–1.55)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.47842+4.63182\text{×}10^{-3}λ^{-2}-8.63733\text{×}10^{-6}λ^{-4}$$

Conditions

temperature: 298

Comments

25 °C

References

Acrylic Matching Liquid Code 5032 Data Sheet 30-NOV-17 (obtained from https://www.cargille.com)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of Acrylic matching liquid

density:
  - 
    temperature: 298
    value: 888
thermal_expansion:
  - 
    temperature: 298
    value: 0.0007

About Index-matching materials

An index-matching material is usually used to create an optical contact with minimum reflection between optical components.