$$n=1.473749+6.5503120\text{×}10^{-3}λ^{-2}-1.2694420\text{×}10^{-5}λ^{-4}$$Conditions
temperature: 298
Comments
25 °C
References
Acrylic Double Matching Liquid Code 4213295 Data Sheet 29-MAR-17 (obtained from https://www.cargille.com)
Data
Additional information
Properties of Acrylic double matching liquid
density: - temperature: 298 value: 1184 thermal_expansion: - temperature: 298 value: 0.00066