Optical constants of CARGILLE
Fused silica matching liquid 06350
Wavelength:
µm
(0.225–1.55)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.44719+3.83343\text{×}10^{-3}λ^{-2}+5.66134\text{×}10^{-5}λ^{-4}$$Conditions
temperature: 298
Comments
25 °C.
References
Fused Silica Matching Liquid Code 06350 Data Sheet 30-NOV-17 (obtained from https://www.cargille.com)
Data
Additional information
Properties of Fused silica matching liquid 06350
density: - temperature: 298 value: 824 thermal_expansion: - temperature: 298 value: 0.0008
About Index-matching materials
An index-matching material is usually used to create an optical contact with minimum reflection between optical components.
Links: