Optical constants of CRYSTRAN - Optical materials
LaF3 - Lanthanum fluoride (o)

Wavelength: µm
 (0.254–15.0)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

orientation: o

Comments

Lanthanum Fluoride is not often used as an optical material. Lanthanum Fluoride is usually doped with Europium at a nominal level of 0.3% mole. In this form, the usual application is as the active element in an ion-selective electrode for the detection and measurement of Fluoride ions in solution.
Lanthanum Fluoride is grown as small ingots of about 10mm diameter as it is difficult to anneal. Doped with Europium, it is a pale yellow colour.
REFERENCES:
(1) Jones and Shand, J.Crys.Growth. 2 (1968) p3611
(2) Sher, Solomon, Lee, and Meuller. Phys.Rev. 144, p593 (1966)
(3) Electronic Processes in Ionic Crystals (OU Press, NY, 1940) p.41 Optical data are for ordinary ray (o).

References

Crystran Ltd. The Crystran handbook of infra-red and ultra-violet optical materials (5th edition, 2023)
See also Crystran LaF3 online data sheet

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of LaF3 - Lanthanum fluoride (o)

density:
  - 
    value: 5940
thermal_expansion:
  - 
    direction: para
    temperature: 298
    value: 1.1E-5
  - 
    direction: perp
    temperature: 298
    value: 1.58E-5
hardness:
  - 
    type: Moh
    value: 4.5
melting_point:
  - 
    value: 1766
thermal_conductivity:
  - 
    temperature: 300
    value: 5.1
solubility:
  - 
    value: 0