Optical constants of CRYSTRAN - optical materials
CsBr
Complex refractive index (n+ik)
Derived optical constants
Conditions
temperature: 300
Comments
Caesium Bromide is grown by sealed ampoule Stockbarger technique. CsBr is a soft pliable material.
IUPAC International Union of Pure and applied Chemistry recommends the spelling as Cesium. UK Useage is Caesium.
Solubility has historically been quoted as 124g/100mL at 25°C but Crystran Ltd tests 2021 have found this to be inaccurate.
REFERENCES:
(1) Handbook Optical Constants, ed Palik, V3, ISBN 0-12-544423-0
(2) Mitsuishi et al., J Opt Soc. Am. V52, p14, 1962
(3) Kelly, Bureau of Mines Bulletin, No371, p51, 1934
(4) S.Ballard et al; J.Opt.Soc.Am. Vol42, p684, 1952
(5) H.H.Li; J.Phys. Chem. Ref. Data. Vol 5, No 2. 1976
(6) K.Matthews. Crystran Ltd Test Data 2021
References
Crystran Ltd.
The Crystran handbook of infra-red and ultra-violet optical materials (5th edition, 2023)
See also
Crystran CsBr online data sheet
Data
Additional information
Properties of CsBr
density: - value: 4400 thermal_dispersion: - type: constant wavelength: 6.0E-7 value: 8.4E-5 thermal_expansion: - temperature: 273 value: 4.79E-5 hardness: - type: Knoop value: 191000000 melting_point: - value: 909 thermal_conductivity: - temperature: 273 value: 0.94 youngs_modulus: - value: 15850000000 poissons_ratio: - value: 0.279 solubility: - temperature: 284 value: 420 - temperature: 288 value: 560 - temperature: 298 value: 900 - temperature: 300 value: 980 - temperature: 301.5 value: 1020 - temperature: 304 value: 1180 - temperature: 308 value: 1380