Optical constants of Amorphous Materials - Infrared glass (AMTIR)
AMTIR-3 (out of production)
Wavelength:
µm
(3–14)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{5.8505λ^2}{λ^2-0.29192^2}+\frac{1.4536λ^2}{λ^2-42.714^2}$$References
Handbook of Optics, Vol. 2, 2nd edition. McGraw-Hill 1994