Optical constants of V-Ga (Vanadium-gallium alloy)
Golovashkin et al. 1970: n,k 0.45-2.6 µm; 78 K

Wavelength: µm
 (0.45 – 2.60)  
 

Derived optical constants

n   k   logX   logY   eV

Comments

78 K (-195 °C). Avaraged data for samples containing 37, 33, and 6 wt% gallium (optical constants of the three samples are close to one another).

References

A. I. Golovashkin, I. S. Levchenko and G. P. Motulevich. Optical properties and electron characteristics of vanadium-gallium alloys obtained by evaporation in vacuum, Sov. Phys. JETP 30, 44-48 (1970)