Optical constants of PTB7:PC71BM
Stelling et al. 2017: n,k 0.302-1.685 µm

Wavelength: µm
 (0.30158 – 1.68492)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Isotropic PTB7:PC71BM thin film (thickness 100 nm) on silicon substrate sandwiched by an silicon oxide (SiO2) layer (thickness 300 nm).

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

C. Stelling, C. R. Singh, M. Karg, T. A. F. König, M. Thelakkat, M. Retsch. Plasmonic nanomeshes: their ambivalent role as transparent electrodes in organic solar cells, Sci. Rep. 7, 42530 (2017) - see Supplementary information (Numerical data kindly provided by Tobias König)

More info - wiki

PTB7:PC71BM

Applications

Chemical composition

PTB7: (C41H53FO4S4)n