RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of P3HT:PC61BM
Stelling et al. 2017: n,k 0.247-1.685 µm

Wavelength: µm
 (0.24718 – 1.68492)  
 

Derived optical constants

n   k   logX   logY   eV

Comments

Isotropic P3HT:PC61BM thin film (thickness 80 nm) on silicon substrate.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

C. Stelling, C. R. Singh, M. Karg, T. A. F. König, M. Thelakkat, M. Retsch. Plasmonic nanomeshes: their ambivalent role as transparent electrodes in organic solar cells, Sci. Rep. 7, 42530 (2017) - see Supplementary information (Numerical data kindly provided by Tobias König)

More info - wiki

P3HT:PC61BM

Applications

Chemical composition

P3HT: (C41H53FO4S4)n

PC61BM: C72H14O2

Other names (P3HT)

Other names (PC61BM)

External links