Optical constants of Norland NOA 61
Norland spec sheet: Cured; n 0.450–1.55 µm
Wavelength:
µm
(0.45 – 1.55)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.5375+0.00829045λ^{-2}-0.000211046λ^{-4}$$References
Norland Optical Adhesive 61 Data 1, Data 2 (accessed 2016-04-20)