Optical constants of Nb:RbTiOPO4 (Niobium-doped rubidium titanyl phosphate, Nb:RTP)
Carvajal et al. 2007: n(β) 0.4-1.5 µm

Wavelength: µm
 (0.4 – 1.5)  
 

Derived optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2=1.1320+\frac{2.0885λ^{2}}{λ^2-0.0278}-0.0096λ^{2}$$

Comments

Rb0.955Ti0.955Nb0.045OPO4; nβ; 293 K (20 °C).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

J. J. Carvajal, P. Segonds, A. Peña, J. Zaccaro, B. Boulanger, F. Díaz and M. Aguiló. Structural and optical properties of RbTiOPO4:Nb crystals , J. Phys.: Condens. Matter 19, 116214, 2007