Optical constants of Nb:RbTiOPO4 (Niobium-doped rubidium titanyl phosphate, Nb:RTP)
Carvajal et al. 2007: n(z) 0.4–1.5 µm
Wavelength:
µm
(0.4–1.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.2619+\frac{1.2069λ^{2}}{λ^2-0.0594}-0.0168λ^{2}$$Conditions
temperature: 293 optical_component: z
Comments
Rb0.955Ti0.955Nb0.045OPO4; nz; 293 K (20 °C).
References
J. J. Carvajal, P. Segonds, A. Peña, J. Zaccaro, B. Boulanger, F. Díaz, M. Aguiló. Structural and optical properties of RbTiOPO4:Nb crystals. J. Phys. Condens. Matter. 19, 116214, 2007
Data
Additional information
About Niobium-doped rubidium titanyl phosphate
Other names and variations
- Nb:RbTiOPO4
- Nb:RTP