Optical constants of NOA-61
Joseph et al. 2020: 1000-nm film; n 0.246-1.69 µm
Wavelength:
µm
(0.2458 – 1.6880)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true film_thickness: 1000 nm substrate: glass
Comments
NOA-61 UV curable resin (Norland Optical Adhesive 61) thin film (thickness 1000 nm) on glass substrate.
References
S. Joseph, S. Sarkar, J. Joseph, Grating-coupled surface plasmon-polariton sensing at a flat metal–analyte interface in a hybrid-configuration, ACS Appl. Mater. Interfaces, 12, 46519-46529 (2020)
(Numerical data kindly provided by Prof. Joby Joseph)