Optical constants of MgO:LiNbO3 (Magnesium oxide doped lithium niobate)
Zelmon et al. 1997: CLN, 5 mol % MgO; n(e) 0.4–5.0 µm

Wavelength: µm
 (0.4–5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{2.2454λ^2}{λ^2-0.01242}+\frac{1.3005λ^2}{λ^2-0.05313}+\frac{6.8972λ^2}{λ^2-331.33}$$

Conditions

temperature: 294
direction: e

Comments

21 °C. Extraordinary ray (e). Congruently grown lithium niobate (CLN) doped with 5 mol. % MgO.
In the original publication, the ordinary and extraordinary Sellmeier coefficients appear to be interchanged. The coefficients are presented here with no and ne swapped to match the measured dispersion and the known negative uniaxial behavior of MgO:LiNbO3.

References

D. E. Zelmon, D. L. Small, D. Jundt. Infrared corrected Sellmeier coefficients for congruently grown lithium niobate and 5 mol.% magnesium oxide-doped lithium niobate. J. Opt. Soc. Am. B 14, 3319-3322 (1997)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Magnesium oxide doped lithium niobate

Other names and variations:
  • MgO:LiNbO3
Links: