Optical constants of Li:C12H4N4 (Lithium:tetracyanoquinodimethane, Li:TCNQ )
Querry 1985: n,k 0.21-55.6 µm

Wavelength: µm
 (0.2100 – 55.5556)  
 

Derived optical constants

n   k   logX   logY   eV

Comments

Lithium:Tetracyanoquinodimethane (Li:TCNQ).

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)