Optical constants of Cu:C12H4N4 (Copper:tetracyanoquinodimethane, Cu:TCNQ )
Querry 1985: n,k 0.21-55.6 µm

Wavelength: µm
 (0.2100 – 55.5556)  
 

Other optical constants

n   k   logX   logY   eV

Comments

Copper:Tetracyanoquinodimethane (Cu:TCNQ).

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)

More info - wiki

Copper:tetracyanoquinodimethane (Cu:TCNQ), Cu:C12H4N4

External links