Optical constants of CsPb(Br,Cl)3 (Cesium lead tribromide - Cesium lead trichloride)
Ermolaev et al. 2023: Br-1.8, Cl-1.2; n,k(o) 0.464–0.700 µm

Wavelength: µm
 (0.464–0.700)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

direction: o

Comments

CsPbBr1.8Cl1.2 monocrystal. Ordinary ray (o).

References

G. Ermolaev, A. P. Pushkarev, A. Zhizhchenko, A. A. Kuchmizhak, I. Iorsh, I. Kruglov, A. Mazitov, A. Ishteev, K. Konstantinova, D. Saranin, A. Slavich, D. Stosic, E. S. Zhukova, G. Tselikov, A. D. Carlo, A. Arsenin, K. S. Novoselov, S. V. Makarov, V. S. Volkov. Giant and tunable excitonic optical anisotropy in single-crystal halide perovskites. Nano Lett. 23, 2570–2577 (2023) (Numerical data kindly provided by Georgy Ermolaev)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Perovskite