Optical constants of (C8H8)n-(C3H3N)m (Styrene-acrylonitrile, SAN)
Sultanova et al. 2009: n 0.4368–1.052 µm

Wavelength: µm
 (0.4368–1.052)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.3787λ^2}{λ^2-0.017842}$$

Conditions

temperature: 293

Comments

20 °C

References

N. Sultanova, S. Kasarova and I. Nikolov. Dispersion properties of optical polymers, Acta Physica Polonica A 116, 585-587 (2009)