Optical constants of (C35H42N2S)n (F8BT)
Kamptner et al. 2024: n,k(o) 0.191–1.69 µm

Wavelength: µm
 (0.19146–1.68869)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

direction: o

Comments

Ordinary ray (o)

References

A. Kamptner, M. C. Scharber, M. Schiek. Accurate determination of the uniaxial complex refractive index and the optical band gap of polymer thin films to correlate their absorption strength and onset of absorption. Chem. Phys. Chem. e202400233 (2024) (Numerical data kindly provided by Manuela Schiek)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About (C35H42N2S)n

Other names and variations:
  • F8BT
  • PFBT
  • Poly(9,9-dioctyluorene-alt-benzothiadiazole)
  • 2,1,3-benzothiadiazole-9,9-dioctylfluorene copolymer
  • 9,9-dioctylfluorene-2,1,3-benzothiadiazole copolymer
  • PFO-BT 15