RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of ZrTe5 (Zirconium pentatelluride)
Guo et al. 2021: n,k(b) 0.193–1.30 µm

Wavelength: µm
 (0.1930–1.3000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

optical_component: b

Comments

nb, kb; room temperature.

References

Z. Guo, H. Gu, M. Fang, B. Song, W. Wang, X. Chen, C. Zhang, H. Jiang, L. Wang, S. Liu. Complete dielectric tensor and giant optical anisotropy in quasi-one-dimensional ZrTe5. ACS Mater. Lett., 3, 6525–6534 (2021) (Numerical data kindly provided by Zhengfeng Guo)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zirconium pentatelluride

Zirconium pentatelluride (ZrTe5) is a layered compound with unique electronic properties, drawing interest in the field of condensed matter physics. Due to its peculiar electronic band structure, it has been investigated as a potential candidate for quantum spin Hall states and topological insulators. Additionally, ZrTe5 exhibits a large, negative magnetoresistance at low temperatures, which makes it a subject of study for potential electronic and spintronic applications. Its intriguing properties continue to be the focus of ongoing research to better understand its potential in various technological applications and the fundamental physics that drive its behavior.

Other names and variations

  • ZrTe5

Links