Optical constants of WTe2 (Tungsten ditelluride)
Munkhbat et al. 2022: multilayer flakes; n(z) 0.30–1.69 µm
Complex refractive index (n+ik)
Derived optical constants
Conditions
optical_component: z
Comments
Multilayer flakes. nz. Room temperature.
References
B. Munkhbat, P. Wrobel, T. J. Antosiewicz, T. O. Shegai. Optical constants of several multilayer transition metal dichalcogenides spectroscopic ellipsometry in the 300–1700 nm range: High index, anisotropy, and hyperbolicity. ACS Photonics 9, 2398–2407 (2022) (Numerical data kindly provided by Tomasz Antosiewicz)
Data
Additional information
About Tungsten ditelluride
Tungsten ditelluride (WTe2) is a member of the transition metal dichalcogenides (TMDs) group, possessing unique electronic properties that set it apart from other TMDs. Characterized by its layered structure, the layers are held together by weak van der Waals forces, making it possible to exfoliate into ultra-thin layers. WTe2 has gained significant attention due to its extremely large magnetoresistance and the discovery of type-II Weyl semimetal state in its structure. The combination of these unusual properties has spurred interest in its potential for advanced electronic, spintronic, and quantum devices. Moreover, its inherent flexibility in thin layers can be advantageous for future wearable or flexible device applications.
Other names and variations
- WTe2
- Tungsten(IV) telluride
Links