Optical constants of Pb (Lead)
Golovashkin and Motulevich 1968: n,k 0.45-12 µm; 293 K

Wavelength: µm
 (0.45 – 12.0)  
 

Derived optical constants

n   k   logX   logY   eV

Comments

293 K (20 °C)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

A. I. Golovashkin and G. P. Motulevich. Optical properties of lead in the visible and infrared spectral ranges, Sov. Phys. JETP 26, 881-887 (1968)