Optical constants of MoS2 (Molybdenum disulfide)
Ermolaev et al. 2020: bulk; n,k 0.290-3.30 µm
Wavelength:
µm
(0.290 – 3.300)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
Comments
Broadband optical constants of in-plane component of dielectric tensor of bulk MoS2 were measured by spectroscopic ellipsometry in the spectral range 290-3300 nm.
References
G. A. Ermolaev, Yu. V. Stebunov, A. A. Vyshnevyy, D. E. Tatarkin, D. I. Yakubovsky, S. M. Novikov, D. G. Baranov, T. Shegai, A. Y. Nikitin, A. V. Arsenin, V. S. Volkov. Broadband optical properties of monolayer and bulk MoS2, NPJ 2D Mater. Appl., 4, 21 (2020) (Numerical data kindly provided by Georgy Ermolaev)