Optical constants of MoO3 (Molybdenum trioxide)
Toksumakov et al. 2025: n,k(b) 0.250–30.0 µm

Wavelength: µm
 (0.250–30.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

optical_component: b

Comments

α-MoO3. Crystallographic b-axis.

References

A. N. Toksumakov, D. V. Grudinin, G. A. Ermolaev, A. P. Tsapenko, A. A. Minnekhanov, K. V. Kravtsov, N. Pak, A. Mazitov, A. A. Vyshnevyy, A. S. Slavich, I. A. Kruglov, G. I. Tselikov, A. V. Arsenin, K. S. Novoselov, V. S. Volkov. Unveiling α-MoO3 as a High-Index, Low-Loss Anisotropic Material: Bridging the Gap from Mid-Infrared to Ultraviolet Nanophotonics. Adv. Mater., e74228 (2026) (See Supporting Information)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Molybdenum trioxide

Molybdenum trioxide (MoO3) is a compound of molybdenum and oxygen. It appears as an odorless, light-colored crystalline solid. It is a primary component in the production of molybdenum metal. In the field of optics, thin films of MoO3 can be deposited on various substrates, serving as layers in certain optoelectronic devices due to its semiconducting properties. The compound is also investigated for potential uses in energy storage and sensor applications. Additionally, its transparency to infrared radiation makes it a candidate for specific optical applications in the IR range.

Other names and variations

  • MoO3
  • Molybdic anhydride
  • Molybdite
  • Molybdic trioxide
  • Molybdenum(VI) oxide

Links