Optical constants of HfO2 (Hafnium dioxide, Hafnia)
Wood et al. 1990: Cubic hafnia; n 0.361-5.135 µm

Wavelength: µm
 (0.365 – 5)  
 

Derived optical constants

logX   logY   eV

Dispersion formula [ i ]

$$n^2-1=\frac{1.9558λ^2}{λ^2-0.15494^2}+\frac{1.345λ^2}{λ^2-0.0634^2}+\frac{10.41λ^2}{λ^2-27.12^2}$$

Comments

Cubic hafnia; 20 °C; Y2O3 content: 9.8 mol. %

References

D. L. Wood, Kurt Nassau, T. Y. Kometani, and D. L. Nash. Optical properties of cubic hafnia stabilized with yttria. Appl. Opt. 29, 604-607 (1990)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]