Optical constants of DyScO3 (Dysprosium scandate)
Chernova et al. 2017: n,k 0.14–1.67 µm
Wavelength:
µm
(1.4089e-01–1.6755e+00)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Single crystal Dysprosium scandate
References
E. Chernova, C. Brooks, D. Chvostova, Z. Bryknar, A. Dejneka, M. Tyunina.
Optical NIR-VIS-VUV constants of advanced substrates for thin-film devices.
Opt. Mater. Express 7, 3844–3862 (2017)
[Calculation script (Python)]
Data
Additional information
About Dysprosium scandate
Dysprosium scandate (DyScO3)
Other names and variations:- DyScO3