Optical constants of BaTiO3 (Barium titanate)
Timpu et al. 2019: n 0.4–0.8 µm

Wavelength: µm
 (3.5000e-01–8.0000e-01)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

film_thickness: 2.2E-7
substrate: glass
deposition_temperature: 923

Comments

Pulsed laser deposition (PLD) grown BaTiO3.

References

F. Timpu, M. R. Escalé, M. Timofeeva, N. Strkalj, M. Trassin, M. Fiebig, R. Grange. Enhanced nonlinear yield from barium titanate metasurface down to the near ultraviolet. Adv. Opt. Mater. 7, 1900936 (2019) (Data points extracted from a figure)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Barium titanate

BaTiO3, or barium titanate, is a ferroelectric crystal with a perovskite structure that is highly prized for its dielectric and piezoelectric properties. In the realm of optics, this material is particularly important for its electro-optic and nonlinear optical capabilities. It exhibits a high refractive index, and its electro-optic coefficients are among the highest of the known crystals, making it well-suited for applications such as optical modulators and beam deflectors. In addition to its electro-optic uses, BaTiO3 is employed in the fabrication of photonic devices like waveguides and resonators. Its ferroelectric nature also enables applications in data storage and other memory devices. BaTiO3 can be grown using various techniques such as the Bridgman or Czochralski methods and can be doped with different elements to fine-tune its properties. While it is a robust and versatile material, it is sensitive to defects and impurities, which can impact its optical performance. Overall, BaTiO3 is a multifunctional material with a wide range of applications in both the electronic and optical domains, making it a subject of continued research and technological development.

Other names and variations:
  • BaTiO3
Links: