RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of BaGa4Se7 (Barium gallium selenide, BGSe)
Badikov et al 2010: n(y) 0.480–10.4 µm

Wavelength: µm
 (0.48–10.4)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=7.323096+\frac{0.292889}{λ^2-0.052725}+\frac{1573.474}{λ^2-1182.324}$$

Conditions

optical_component: true

Comments

ny; room temperature.

References

V. Badikov, D. Badikov, G. Shevyrdyaeva, A. Tyazhev, G. Marchev, V. Panyutin, V. Petrov, A. Kwasniewski. Phase-matching properties of BaGa4S7 and BaGa4Se7: Wide-bandgap nonlinear crystals for the mid-infrared. Phys. Status Solidi RRL, 5, 31–33 (2010)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About BaGa4Se7

BaGa4Se7, commonly abbreviated as BGSe, is a chalcogenide-based nonlinear optical crystal known for its phase-matching capabilities and broad transparency window. This material is particularly suited for frequency conversion applications in the mid-infrared region, including second-harmonic generation (SHG), sum-frequency generation (SFG), and optical parametric oscillation (OPO). BGSe exhibits high nonlinear optical coefficients, as well as a high laser damage threshold, making it well-suited for high-power applications. The crystal is generally grown using techniques like the Bridgman-Stockbarger method, and can be cut and polished into high-quality facets for optimal performance. One important consideration for this material is its sensitivity to moisture and other environmental factors; thus, careful handling and storage are required to maintain its optical properties. Overall, BGSe offers a compelling combination of properties that make it a valuable material for nonlinear optics, especially for applications requiring high efficiency and broad tunability in the mid-infrared range.