RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of As2S3 (Arsenic trisulfide)
Slavich et al. 2024: Ab initio; n,k(b) 0.299–2.07 µm

Wavelength: µm
 (0.29875–2.07115)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

optical_component: b

Comments

Crystallographic b-axis. Ab initio calculations.

References

A. S. Slavich, G. A. Ermolaev, M. K. Tatmyshevskiy, A. N. Toksumakov, O. G. Matveeva, D. V. Grudinin, K. V. Voronin, A. Mazitov, K. V. Kravtsov, A. V. Syuy, D. M. Tsymbarenko, M. S. Mironov, S. M. Novikov, I. Kruglov, D. A. Ghazaryan, A. A. Vyshnevyy, A. V. Arsenin, V. S. Volkov, K. S Novoselov. Exploring van der Waals materials with high anisotropy: geometrical and optical approaches. Light Sci. Appl., 13, 68 (2024) (Numerical data kindly provided by Georgy Ermolaev)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Arsenic trisulfide

As2S3, also known as arsenic trisulfide, exists in both crystalline and amorphous forms. The crystalline form is commonly referred to as orpiment and occurs naturally as a mineral. However, in optical and photonic applications, the amorphous or glassy form of As2S3 is often preferred. This chalcogenide glass features a broad transmission window that extends from the visible to the mid-infrared spectral regions, and it is known for its high nonlinear optical coefficients. The amorphous structure allows for the material to be easily molded, drawn into fibers, or deposited as thin films, making it highly versatile for a variety of optoelectronic applications. It also offers the advantage of strong light confinement due to its high refractive index. However, users should exercise caution as the material contains toxic arsenic, and its photosensitive nature necessitates consideration for stability under light exposure. Whether in its crystalline or amorphous state, As2S3 remains a material of significant interest for both its unique optical properties and its potential in emerging technologies.

Mineral: Orpiment

Other names and variations

  • As2S3
  • Arsenic(III) sulfide
  • Diarsenic trisulfide
  • Arsenic trisulphide
  • Arsenic(III) sulphide
  • Diarsenic trisulphide
  • Orpiment

Links