Optical constants of SUMITA - Glasses for precision molding
K-ZnSF8

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.8600337-1.2073452\text{×}10^{-2}λ^{2}+2.6131306\text{×}10^{-2}λ^{-2}+9.1303268\text{×}10^{-4}λ^{-4}-3.0467767\text{×}10^{-5}λ^{-6}+4.891802\text{×}10^{-6}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book

More info - wiki

-