Optical constants of SUMITA - Glasses for precision molding
K-VC90

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.3299316-1.3661207\text{×}10^{-2}λ^{2}+3.4088332\text{×}10^{-2}λ^{-2}+1.0979548\text{×}10^{-3}λ^{-4}-2.7983676\text{×}10^{-5}λ^{-6}+5.172898\text{×}10^{-6}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book