K-VC82

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.0092545-1.4428442\text{×}10^{-2}λ^{2}+2.4950143\text{×}10^{-2}λ^{-2}+6.532589\text{×}10^{-4}λ^{-4}-1.7536585\text{×}10^{-5}λ^{-6}+2.6440099\text{×}10^{-6}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.