Optical constants of SUMITA - Glasses for precision molding
K-VC79

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.5520489-1.1234947\text{×}10^{-2}λ^{2}+1.4455084\text{×}10^{-2}λ^{-2}+4.6725318\text{×}10^{-4}λ^{-4}-3.6714004\text{×}10^{-5}λ^{-6}+2.2810504\text{×}10^{-6}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

References

Sumita Optical Glass Data Book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]