RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of SUMITA - Glasses for precision molding
K-VC78

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.7376882-1.2269245\text{×}10^{-2}λ^{2}+1.7439403\text{×}10^{-2}λ^{-2}+4.7088707\text{×}10^{-4}λ^{-4}-2.7150134\text{×}10^{-5}λ^{-6}+1.8172045\text{×}10^{-6}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book

More info - wiki

-