Optical constants of SUMITA - Glasses for precision molding
K-SKF6

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.2505164-8.8684142\text{×}10^{-3}λ^{2}+1.2260534\text{×}10^{-2}λ^{-2}+4.2234633\text{×}10^{-4}λ^{-4}-2.1095054\text{×}10^{-5}λ^{-6}+2.2440064\text{×}10^{-6}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

References

Sumita Optical Glass Data Book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]