Optical constants of SUMITA - Glasses for precision molding
K-PSFn202

Wavelength: µm
 (0.365 – 1.548)  
 

Derived optical constants

logX   logY   eV

Dispersion formula

$$n^2=3.8508789-1.6529344\text{×}10^{-2}λ^{2}+6.6096066\text{×}10^{-2}λ^{-2}+5.8480521\text{×}10^{-3}λ^{-4}-5.055984\text{×}10^{-4}λ^{-6}+7.6558669\text{×}10^{-5}λ^{-8}$$

Comments

Glass for Precision Molding. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Sumita Optical Glass Data Book